Pelepas acuan — pilihan mengikut resin
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Lihat butiran
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Berikan model mesin, ton atau ruang sedia ada. Kami sahkan unit tepat, kawalan dan pilihan sebelum menawarkan harga.
Ulasan kejuruteraan Isnin hingga Sabtu. Berikan model mesin dan pengeluaran yang diperlukan — jawapan membawa harga, skop dan penghantaran.
Pengering, penyejuk, penghancur dan seluruh sel acuan, dikonfigurasi mengikut susun atur kilang dan peralatan sedia ada anda.
Tidak pasti saiz mana sesuai? Hantar model mesin atau foto unit sedia ada dan kami padankan.
A mold release is the cheapest tool you have against sticking parts, ejector pin marks and short shots caused by drag. The right grade depends less on the resin than on what happens after ejection — whether the part gets painted, printed, welded or bonded.
| Type | Carrier | Best for | Finishing compatibility |
|---|---|---|---|
| Silicone | Solvent | Deep draws, textured molds, long runs | Must be removed before painting |
| Non-silicone | Solvent | Parts that will be painted, printed or bonded | Painting and assembly safe |
| Water-based | Water | Operator safety, low VOC workshops | Good, low residue |
| Dry film | Solvent | Semi-permanent release, high volume | Usually needs stripping before finishing |
| Silicone-free paste | Grease | Localized trouble spots, hot runner drops | Apply sparingly |
Most release problems are application problems. Spray from 200 - 300 mm at a 45 degree angle, let the carrier flash off, and apply to a mold between 40 and 80 °C — not to a cold mold, where the film pools in the corners. One light pass every five to twenty shots is normally enough. Over-application causes splay, silver streaking and paint adhesion failures far more often than under-application.
For polycarbonate and other transparent resins, use the non-silicone grade and reduce quantity; silicone contamination shows up as haze that cannot be polished out. For POM and PA with deep cores, a silicone grade gives better release but requires a proper washing step before any secondary operation.
Tell us your resin and what happens to the part after molding and we will recommend the grade and pack size.
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Lihat butiranBerikan model mesin dan resin — kami sahkan geometri, bahan dan rawatan sebelum menawarkan harga.
Ada lukisan? Balas emel pengesahan kami dengan fail dilampirkan — PDF, STEP, DXF atau foto bahagian semuanya boleh.
Pasukan kejuruteraan kami menjawab dalam waktu bekerja, Isnin hingga Sabtu. Untuk pesanan segera, hubungi +8613751260808.