Desmoldantes — elección según resina
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Ver detalles
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Indíquenos el modelo de máquina, la tonelada o el espacio disponible. Confirmamos la unidad exacta, los controles y las opciones antes de cotizar.
Revisión de ingeniería de lunes a sábado. Envíe el modelo de máquina y la producción que necesita — la respuesta incluye precio, alcance y entrega.
Secadores, enfriadores, granuladores y el resto de la celda de moldeo, configurados según su planta y su equipo existente.
¿No sabe qué medida encaja? Envíe el modelo de máquina o una foto del equipo existente y lo emparejamos.
A mold release is the cheapest tool you have against sticking parts, ejector pin marks and short shots caused by drag. The right grade depends less on the resin than on what happens after ejection — whether the part gets painted, printed, welded or bonded.
| Type | Carrier | Best for | Finishing compatibility |
|---|---|---|---|
| Silicone | Solvent | Deep draws, textured molds, long runs | Must be removed before painting |
| Non-silicone | Solvent | Parts that will be painted, printed or bonded | Painting and assembly safe |
| Water-based | Water | Operator safety, low VOC workshops | Good, low residue |
| Dry film | Solvent | Semi-permanent release, high volume | Usually needs stripping before finishing |
| Silicone-free paste | Grease | Localized trouble spots, hot runner drops | Apply sparingly |
Most release problems are application problems. Spray from 200 - 300 mm at a 45 degree angle, let the carrier flash off, and apply to a mold between 40 and 80 °C — not to a cold mold, where the film pools in the corners. One light pass every five to twenty shots is normally enough. Over-application causes splay, silver streaking and paint adhesion failures far more often than under-application.
For polycarbonate and other transparent resins, use the non-silicone grade and reduce quantity; silicone contamination shows up as haze that cannot be polished out. For POM and PA with deep cores, a silicone grade gives better release but requires a proper washing step before any secondary operation.
Tell us your resin and what happens to the part after molding and we will recommend the grade and pack size.
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Ver detallesIndique el modelo de máquina y la resina — confirmamos geometría, material y tratamiento antes de cotizar.
¿Tiene el plano? Responda a nuestro correo de confirmación con el archivo adjunto — valen PDF, STEP, DXF o una foto de la pieza.
Nuestro equipo de ingeniería responde en horario laboral, de lunes a sábado. Para pedidos urgentes, llame al +8613751260808.