Agents démoulants — choix selon la résine
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Voir le détail
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Indiquez-nous le modèle de machine, la force de fermeture ou l’encombrement. Nous confirmons l’unité exacte, les commandes et les options avant de chiffrer.
Revue d’ingénierie du lundi au samedi. Indiquez le modèle de machine et le débit souhaité — la réponse comporte prix, périmètre et délai.
Sécheurs, refroidisseurs, granulateurs et le reste de la cellule, configurés selon votre atelier et votre équipement actuel.
Vous ne savez pas quelle taille convient ? Envoyez le modèle de machine ou une photo de l’équipement existant, nous l’apparierons.
A mold release is the cheapest tool you have against sticking parts, ejector pin marks and short shots caused by drag. The right grade depends less on the resin than on what happens after ejection — whether the part gets painted, printed, welded or bonded.
| Type | Carrier | Best for | Finishing compatibility |
|---|---|---|---|
| Silicone | Solvent | Deep draws, textured molds, long runs | Must be removed before painting |
| Non-silicone | Solvent | Parts that will be painted, printed or bonded | Painting and assembly safe |
| Water-based | Water | Operator safety, low VOC workshops | Good, low residue |
| Dry film | Solvent | Semi-permanent release, high volume | Usually needs stripping before finishing |
| Silicone-free paste | Grease | Localized trouble spots, hot runner drops | Apply sparingly |
Most release problems are application problems. Spray from 200 - 300 mm at a 45 degree angle, let the carrier flash off, and apply to a mold between 40 and 80 °C — not to a cold mold, where the film pools in the corners. One light pass every five to twenty shots is normally enough. Over-application causes splay, silver streaking and paint adhesion failures far more often than under-application.
For polycarbonate and other transparent resins, use the non-silicone grade and reduce quantity; silicone contamination shows up as haze that cannot be polished out. For POM and PA with deep cores, a silicone grade gives better release but requires a proper washing step before any secondary operation.
Tell us your resin and what happens to the part after molding and we will recommend the grade and pack size.
Mold release agents for injection molding in silicone, non-silicone, water-based and solvent-based grades, aerosol and bulk, for PC, PA, POM and textured...
Voir le détailIndiquez le modèle de machine et la résine — nous confirmons géométrie, matériau et traitement avant de chiffrer.
Vous avez un plan ? Répondez à notre e-mail de confirmation avec le fichier — PDF, STEP, DXF ou photo de la pièce, tout convient.
Notre équipe d’ingénierie répond aux heures ouvrées, du lundi au samedi. Pour les commandes urgentes, appelez le +8613751260808.