Dongguan International Technology Transfer Center, 124 Dongbao Road, Dongcheng District, Dongguan, China
Request a quote
Barrier Screw for Better Melt Quality
Screws for Injection Molding

Barrier Screw for Better Melt Quality

Separates solids from melt for a more even melt temperature on large shots and narrow processing windows.

Made to your drawing, sample or part number

Machined to your barrel dimensions and screw geometry — no catalogue constraints. Single replacement part or production batch.

Quoted to confirmed specs

Engineering review Monday to Saturday. Send the machine model, screw diameter and resin — the reply carries price, material grade and lead time.

Email engineering

No drawing on file? Send a photo of the worn part and the machine model — we work the geometry back and confirm it with you before machining.

Details

Specification & application

A barrier screw separates what a general purpose screw cannot: it keeps solid resin and already melted polymer apart along the whole melting length. A secondary flight runs beside the main flight, the solid bed is trapped in the channel it leaves, and melt that forms is forced over the barrier into the metering channel.

The result is a melt that is fully plasticized at a lower average temperature, because the solid is not being dragged through a melt pool that is already hot.

Geometry

ParameterTypical rangeNote
Screw diameterMatched to your barrel boreBarrier screws are cut per order, not stocked
L/D ratioFrom about 24:1 upward, depending on output targetLonger screws give the barrier zone room to work
Barrier flight clearanceA few hundredths of a millimeter over the main flightToo much and the solid bed leaks past; too little and it scores the barrel
Barrier flight leadSet against the main flight pitchControls how fast the melt is drawn off the solid bed
Compression ratioOften lower than a general purpose screwThe barrier does the work; excessive compression adds shear heat

Where it earns its cost

  • Thick-walled parts and large shot weights, where a three-zone screw leaves unmelted cores.
  • High output demands on a fixed cycle — the recovery time drops noticeably.
  • Engineering resins with a narrow processing window, where melt temperature variation shows up as dimensional scatter.
  • Glass-filled grades, where the gentler melt history reduces fiber breakage.

Trade-offs you should know about

  • The extra flight makes the screw harder to clean. Color changes take longer than on a general purpose screw.
  • Wear is concentrated on the barrier flight, so the surface treatment matters more than it does on a three-zone screw.
  • A barrier screw does not fix a bad temperature profile. If the barrel heaters are uneven, the melt will still be uneven.

We size the barrier zone against your output target and resin, and confirm the profile on a drawing before cutting.

Related

Other components in this range

View category

Need this part matched to your press?

Send the machine model and the resin. We confirm geometry, material and surface treatment before quoting.

Barrier Screw for Better Melt Quality Quoted to confirmed specs