仕様と用途
A nitrided barrel is the standard economical construction: a 38CrMoAlA tube, bored and honed, then gas nitrided so the bore carries a hard case over a tough core. The case resists abrasion; the core keeps the barrel from cracking under hoop stress.
Construction data
| Parameter | Typical range | Confirmed at order |
|---|---|---|
| Base material | 38CrMoAlA (JIS SACM645) or equivalent | Mill certificate supplied on request |
| Case depth | Commonly 0.3 to 0.6 mm on the bore | Measured on a test coupon from the same batch |
| Surface hardness | Commonly HRC 56 to 58 band | Verified after nitriding |
| Bore finish | Honed, typically Ra 0.4 µm or better | Checked with a profilometer before dispatch |
| Straightness | Controlled along the full length | Dial-checked on the bench |
| Bore tolerance | Set against the screw clearance | Agreed on the drawing |
What it handles well
- Unfilled commodity resins: PP, PE, PS, ABS, and their blends.
- General purpose and barrier screws in the same barrel material.
- Applications where the budget matters and the filler content is low or zero.
Where it falls short
- Glass and mineral filled compounds. The filler abrades the case faster than the case can resist, and once the case is through, wear accelerates.
- Corrosive resins and PVC, where the nitride layer offers no chemical protection.
- Very long uninterrupted runs on abrasive material — a bimetallic liner will outlast it.
Making it last
Most nitrided barrels we replace were not worn out by the resin. They were worn out by heat: a drifting thermocouple that ran the zone hot softened the case, and after that the wear is rapid. Check the heater bands and thermocouples before blaming the barrel.
Frequently asked questions
Can a nitrided barrel run glass-filled compounds?
For short runs, yes. Under continuous abrasive filler the case wears through faster and the bore loses tolerance — for regular filled work, a bimetallic barrel is the better investment.
The bore of my barrel is worn oversize. Can it be fixed?
Measure first. Nitriding builds a thin hard case — it does not restore a worn bore. If the bore is out of tolerance it has to be re-machined, which changes the clearance against the screw; at that point a new matched screw-and-barrel set is often the more economical route. We quote against the measured bore.
What nitride case depth and hardness do you deliver?
The bore carries a gas-nitrided case with the core staying tough. Case depth and surface hardness are measured on same-batch coupons that accompany the order, and the figures are recorded in the inspection record shipped with the barrel.
Do you machine the feed throat and nozzle end to my machine?
Yes. Feed opening, heater band layout and nozzle bore are machined to the machine's configuration — send the machine model or the old barrel.