Cilindro bimetálico para compuestos con vidrio
Wear-resistant liner for glass-filled, mineral-filled and abrasive compounds.
Ver detalles
Hardened bore for commodity and engineering resins without aggressive fillers.
Mecanizado según las dimensiones de su cilindro y la geometría de su tornillo — sin límites de catálogo. Pieza de repuesto unitaria o lote de producción.
Revisión de ingeniería de lunes a sábado. Envíe el modelo de máquina, el diámetro del tornillo y la resina — la respuesta incluye precio, grado de material y plazo de entrega.
Mecanizamos por dimensiones, no por catálogo — tornillos y cilindros de repuesto para Haitian, Engel, Husky, Arburg, Nissei y otras máquinas, adaptados al diámetro interior medido y a la conexión de accionamiento.
¿No tiene el plano? Envíe una foto de la pieza desgastada y el modelo de máquina — reconstruimos la geometría y la confirmamos con usted antes de mecanizar.
A nitrided barrel is the standard economical construction: a 38CrMoAlA tube, bored and honed, then gas nitrided so the bore carries a hard case over a tough core. The case resists abrasion; the core keeps the barrel from cracking under hoop stress.
| Parameter | Typical range | Confirmed at order |
|---|---|---|
| Base material | 38CrMoAlA (JIS SACM645) or equivalent | Mill certificate supplied on request |
| Case depth | Commonly 0.3 to 0.6 mm on the bore | Measured on a test coupon from the same batch |
| Surface hardness | Commonly HRC 56 to 58 band | Verified after nitriding |
| Bore finish | Honed, typically Ra 0.4 µm or better | Checked with a profilometer before dispatch |
| Straightness | Controlled along the full length | Dial-checked on the bench |
| Bore tolerance | Set against the screw clearance | Agreed on the drawing |
Most nitrided barrels we replace were not worn out by the resin. They were worn out by heat: a drifting thermocouple that ran the zone hot softened the case, and after that the wear is rapid. Check the heater bands and thermocouples before blaming the barrel.
For short runs, yes. Under continuous abrasive filler the case wears through faster and the bore loses tolerance — for regular filled work, a bimetallic barrel is the better investment.
Measure first. Nitriding builds a thin hard case — it does not restore a worn bore. If the bore is out of tolerance it has to be re-machined, which changes the clearance against the screw; at that point a new matched screw-and-barrel set is often the more economical route. We quote against the measured bore.
The bore carries a gas-nitrided case with the core staying tough. Case depth and surface hardness are measured on same-batch coupons that accompany the order, and the figures are recorded in the inspection record shipped with the barrel.
Yes. Feed opening, heater band layout and nozzle bore are machined to the machine's configuration — send the machine model or the old barrel.
Wear-resistant liner for glass-filled, mineral-filled and abrasive compounds.
Ver detalles
Cilindros para máquinas de inyección y extrusión con camisa nitrurada o bimetálica, mecanizados según las dimensiones de su tornillo e inspeccionados contra plano.
Ver detalles
Hardened bore for commodity and engineering resins without aggressive fillers.
Ver detallesIndique el modelo de máquina y la resina — confirmamos geometría, material y tratamiento antes de cotizar.
¿Tiene el plano? Responda a nuestro correo de confirmación con el archivo adjunto — valen PDF, STEP, DXF o una foto de la pieza.
Nuestro equipo de ingeniería responde en horario laboral, de lunes a sábado. Para pedidos urgentes, llame al +8613751260808.