Dongguan, Guangdong, China
Minta sebut harga
Skru penghalang untuk kualiti leburan lebih baik
Skru untuk suntikan

Skru penghalang untuk kualiti leburan lebih baik

Separates solids from melt for a more even melt temperature on large shots and narrow processing windows.

Dibina mengikut lukisan, sampel atau nombor bahagian anda

Diproses mengikut dimensi silinder dan geometri skru anda — tanpa sekatan katalog. Satu bahagian gantian atau lot pengeluaran.

Ditawarkan mengikut spesifikasi yang disahkan

Ulasan kejuruteraan Isnin hingga Sabtu. Hantar model mesin, diameter skru dan resin — jawapan membawa harga, gred bahan dan masa penghantaran.

Untuk semua jenama mesin

Kami memproses mengikut dimensi, bukan katalog — skru dan silinder gantian untuk Haitian, Engel, Husky, Arburg, Nissei dan mesin lain, dipadankan dengan lubang terukur dan sambungan pemacu.

Email kejuruteraan

Tiada lukisan? Hantar foto bahagian yang haus dan model mesin — kami kira balik geometri dan sahkan dengan anda sebelum pemprosesan.

Butiran

Spesifikasi & aplikasi

A barrier screw separates what a general purpose screw cannot: it keeps solid resin and already melted polymer apart along the whole melting length. A secondary flight runs beside the main flight, the solid bed is trapped in the channel it leaves, and melt that forms is forced over the barrier into the metering channel.

The result is a melt that is fully plasticized at a lower average temperature, because the solid is not being dragged through a melt pool that is already hot.

Geometry

ParameterTypical rangeNote
Screw diameterMatched to your barrel boreBarrier screws are cut per order, not stocked
L/D ratioFrom about 24:1 upward, depending on output targetLonger screws give the barrier zone room to work
Barrier flight clearanceA few hundredths of a millimeter over the main flightToo much and the solid bed leaks past; too little and it scores the barrel
Barrier flight leadSet against the main flight pitchControls how fast the melt is drawn off the solid bed
Compression ratioOften lower than a general purpose screwThe barrier does the work; excessive compression adds shear heat

Where it earns its cost

  • Thick-walled parts and large shot weights, where a three-zone screw leaves unmelted cores.
  • High output demands on a fixed cycle — the recovery time drops noticeably.
  • Engineering resins with a narrow processing window, where melt temperature variation shows up as dimensional scatter.
  • Glass-filled grades, where the gentler melt history reduces fiber breakage.

Trade-offs you should know about

  • The extra flight makes the screw harder to clean. Color changes take longer than on a general purpose screw.
  • Wear is concentrated on the barrier flight, so the surface treatment matters more than it does on a three-zone screw.
  • A barrier screw does not fix a bad temperature profile. If the barrel heaters are uneven, the melt will still be uneven.

We size the barrier zone against your output target and resin, and confirm the profile on a drawing before cutting.

Berkaitan

Komponen lain dalam rangkaian ini

Lihat kategori

Perlu bahagian ini dipadankan dengan mesin anda?

Berikan model mesin dan resin — kami sahkan geometri, bahan dan rawatan sebelum menawarkan harga.

Skru penghalang untuk kualiti leburan lebih baik Ditawarkan mengikut spesifikasi yang disahkan